Hello
I am student at a school for polymer technology and would like to use your tutorial in my project work at school. I have some additional questions concerning your tutorial and these are :
-What type of resin is the resin in Unimold system, for example epoxy?
-With what is the coupling coat in Unimold system reinforced? just simply, nothing, glass, carbon,...
-How much IN2 resin we need for the each infusion, we have the ratio numbers but there are no informations about the quantity?
-Price including everything
We need to fully present the process, materials, quantities, so I would be grateful for your reply.
Thank you