Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
I agree you just havent polished it enough yet. What grit did you sand to before compounding? 1200 grit is sort of the bare minimum you want to start from, and it can actually take a lot of compounding to polish up to a real full gloss. Especially if you are trying to polish epoxy rather than a urethane or polyester, as epoxies are very hard wearing and can take a lot to polish. Some of them will never polish to a full gloss, but modern ones should so I doubt that is your issue.
Personally, I actually sand all the way up to 4000 grit. From here it is much faster to compound to a full gloss and you dont use as much compound.
|