Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
Fasta is spot on with this one. The layer of fibreglass will give it a good degree of toughness making it harder to accidentally press through the thin layer of resin.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|