Yes, Steve, but the mould isn't suspended in a 10m pool. This would actually work like an autoclave without heat, if you bag the mould and evacuate the air. The mould is just filled with water. And this will not work, because of the reasons I mentioned earlier.

Steve Broad
Steve Broad
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
oekmont - 10/1/2018 9:33:18 AM
Yes, Steve, but the mould isn't suspended in a 10m pool. This would actually work like an autoclave without heat, if you bag the mould and evacuate the air. The mould is just filled with water. And this will not work, because of the reasons I mentioned earlier.

Filling the mould with water certainly wouldn't work, which is why I said you need 10m of head :-) Pretty academic, anyway as it isn't gong to happen.