Companies that can CNC 2mm carbon fibre sheet from drawings


Author
Message
Sailing
S
Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)
Group: Forum Members
Posts: 4, Visits: 6
Having built some prototypes using your carbon fibre sheet, I need to get some parts CNC machined in 2mm single sided carbon fibre.  Can you recommend companies that can do this?

Replies
oekmont
oekmont
Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
There are many companies who could mill that, except for the perfect inner corners of course, these aren't possible with cnc routing.
Many companies who sell carbon plates also sell routing services. The central question will be where you're from.

Sailing
S
Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)
Group: Forum Members
Posts: 4, Visits: 6
oekmont - 9/22/2018 5:05:13 PM
There are many companies who could mill that, except for the perfect inner corners of course, these aren't possible with cnc routing.
Many companies who sell carbon plates also sell routing services. The central question will be where you're from.


In the south east UK
GO