This may be a stupid question for you guys, but I'm in need of a material that I can use to mold a curved edging of a tank. The tank is wrapped in pond liner, and the curved edge will be on top of the pond liner. The edge will have a radius of 4 feet (but a half circle) with a height of 1' 2". Here is an image of what I'm talking about - https://prnt.sc/kviqyt

Were thinking of using some sort of silicon glue to glue it to the pond liner, though the seal itself does not need to be 100% water tight.
Andrew Hickman
Andrew Hickman
Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)
Group: Forum Members
Posts: 3, Visits: 9
A good material might be something that can be heated and bent to the desired shape?
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Polypropylene should do that quite easily, but you may find it tricky to bond to. A silicone adhesive might stick, but I'm not sure.
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
Core flute board? 




Andrew Hickman
Andrew Hickman
Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)
Group: Forum Members
Posts: 3, Visits: 9
Fasta - 9/18/2018 2:00:51 AM
Core flute board? 

I'll try it out, thanks!

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search