Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
The simplest way would be a wet lay compression mould. In effect you are taking a mould of each side, wet laying in the fabric and clamping them both together. You want to make the moulds quite sturdy. You could simply fold metal as both surfaces look flat. You would polish highly and in effect "score" around the part on the surface to give a visible cut line.