Question on making plug from pictured piece


Author
Message
drippy
drippy
Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)
Group: Forum Members
Posts: 32, Visits: 388
Image result for integra cargo cover

Interesting situation. I used to make this product in carbon 10 or so years ago but the plug was made for me. This is a cargo cover for a vehicle and it made from that kinda weird pressed cardboard or wood of some sort. It then was sprayed with some fabric on it that doesn't come off.  What is the best approach of making a plug from it. I have plenty of infusion experience but not much in plug making.  I can do all the flanges and stuff no issue just getting this product to that point. Here are some old pics of it when I was making them. The mold is gone that I used cause the company I was making them for paid for the molds so they were exclusive. That company has been gone for like 7 years and I have to chance to sell another batch.



Edited 8 Years Ago by drippy
drippy
drippy
Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)
Group: Forum Members
Posts: 32, Visits: 388


Only picture and pretty terrible at that of the original mold I could find (again 10 years ago). It is hiding in the bottom right of the picture.  Looks like I was masking it off getting it ready for the clear gelcoat.
Edited 8 Years Ago by drippy
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
How does the fluff respond to a flap wheel?  You could skim over it if it helps smooth the surface then coat with some Pattern-Coat Primer



Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Fasta
Fasta
Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
Warren (Staff) - 8/13/2018 8:24:51 AM
How does the fluff respond to a flap wheel?  You could skim over it if it helps smooth the surface then coat with some Pattern-Coat Primer


I was thinking the same and have done this.

Just impregnate the fluff with a primer and sand it smooth. Spray again if needed.





Lester Populaire
L
Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
I would probably put it in an envelope bag and pull a vacuum, pull the bag tight on the whole surface so there aren't plies and take a quick mold on this and then go from there.
drippy
drippy
Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)
Group: Forum Members
Posts: 32, Visits: 388
Fasta - 8/13/2018 8:55:35 AM
Warren (Staff) - 8/13/2018 8:24:51 AM
How does the fluff respond to a flap wheel?  You could skim over it if it helps smooth the surface then coat with some Pattern-Coat Primer


I was thinking the same and have done this.

Just impregnate the fluff with a primer and sand it smooth. Spray again if needed.

This seems like the easiest method. I think years ago I did a headliner where I just saturated it with resin. Sanded it semi smooth and just used filler to completely smooth it out. Was seeing if there is any easier way. I have a couple of these cover and might try just the primer and sanding and also try and use a flap wheel on another to see if it knocks the fluff off.  Is there a specific primer to use? I have some duratec primer which I assume should work fine.

Thanks again for all your help guys!

drippy
drippy
Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)
Group: Forum Members
Posts: 32, Visits: 388
Fasta.. Thanks for the suggestion and it worked perfectly! Took me 2 coats but worked just like I needed it.
Fasta
Fasta
Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
Did you also add some board flange areas to it?




drippy
drippy
Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)
Group: Forum Members
Posts: 32, Visits: 388
Fasta - 8/17/2018 2:25:10 AM
Did you also add some board flange areas to it?

Mold is already done and ready for infusion. It was a nice change of pace making the plug.