Good morning,

I'm working on a a small plug which is about 20" by 25" by 8" deep. Photo hopefully attached. I am planning on sealing the mdf with shellac, then coating it with Duratec. It would be simpler to roll it or brush it, unless that results in a lot of sanding. The downside to spraying (for me) is that I have to purchase a spray gun, and set up a lot of plastic sheeting to contain overspray. Also, I'm wondering if spraying the inside corners of a box shape will result in drips, and end up requiring just at much sanding as brushing it.

I'm a complete newb at this. This is the first plug I've made. In the picture, the white/black stripe is the window flange of a Jeep Wrangler hardtop. The part will be a box that inserts where the window used to be. Later, a hinged cover will be made for the box. 

Thank your for your thoughts on this.
 
Reply
drippy
drippy
Supreme Being (289 reputation)Supreme Being (289 reputation)Supreme Being (289 reputation)Supreme Being (289 reputation)Supreme Being (289 reputation)Supreme Being (289 reputation)Supreme Being (289 reputation)Supreme Being (289 reputation)Supreme Being (289 reputation)
Group: Forum Members
Posts: 32, Visits: 388
I've brushed it before and it does take a couple coats cause it's thin. I ended up getting a $20 spray gun from harbor freight to use just for this application. It works OK for a very cheap gun but still better than brushing
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
DaVikes - 7 Years Ago
Hanaldo - 7 Years Ago
Fasta - 7 Years Ago
Fasta - 7 Years Ago
DaVikes - 7 Years Ago
Fasta - 7 Years Ago
drippy - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search