Group: Forum Members
Posts: 155,
Visits: 992
|
I'll be milling some moulds out of epoxy. I would love to try the s120 sealer but it's just too expensive to ship to the states. Does anyone know of something similar I can get here? Also I'm curious what type of epoxy/filler will work nicely for this? I will probably be building up a layer of epoxy over pre milled mdf leaving a few mm thickness for epoxy and milling final shape into that. Already tried bondo and that works, but I think epoxy/filler will work nicer and be tougher, just not sure what to use. Another guy mentioned coating the mould in Teflon tape which i might consider, but I want to see what is available to use that is similar to s120.
|