how should i tackle this helicopter boom?


Author
Message
quinn
q
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 155, Visits: 992
hello everyone, im new to this forum as well as working with composites. I am designing and building performance rc helicopters using fusion 360 and a cnc that i designed and built. i have already finished my first prototype 700 class (700mm blades) heli and it was a huge success but there are a couple improvements i would like to make. One slight issue the heli has is tail vibrations at very high rpm. currently for the tail boom i am using roll wrapped 1mm wall, 0/90 degree carbon fiber tube. It is 30mm OD and 800mm long. it has excellent bending strength but because of the 0/90 weave, it is lacking in torsional stiffness which i am convinced is allowing the vibrations at higher rpm. I have actually confirmed this before by trying the same kind of tube on other existing heli designs which had an aluminum boom as stock. In my opinion, the solution is adding 45 degree weave with a braided sleeve to give it torsional strength. Using aluminum is another option but for best performance possible, weight is very important and use of carbon fiber is certainly going to make a lighter part for same strength. Easiest solution would be reinforcing an existing tube with braided sleeve on the inner or outer surface but i would like to take it one step further. usually these booms are braced by 2 rod supports at an angle reaching about 2/3 of the way down the boom, but a couple of manufacturers have made heavier duty tapered carbon fiber booms that dont need boom supports. Overall it looks better and can save even more weight. this is what i would like to do on my heli. I have attached 2 pics, one of the whole heli with the tapered boom on it, and the boom by itself. the boom is 800mm long, 30mm diameter out at the end and 40mm wide by 48mm tall at the base. this isnt the final design, i just quickly modeled it to give a representation of what it will be similar too. I am thinking most of it will be about 1mm thick wall with some extra layers at the base to bring it up to 1.5mm or so. fasteners will pass through the wall of the boom and thread into aluminum pieces placed against the inner wall of the boom so the boom wall is clamped against the side frames of the heli. 

so here are my questions. Considering i have a cnc at my disposal, what method is going to give the best results for an efficient part? As i mentioned, weight is very important so every gram counts, which means i would like to have as low of ratio possible of resin vs carbon fiber. since i need to have continuous 45 degree weave for torsional strength, that means i need to use braided sleeve which im sure complicates things since i cant just join 2 mold halves together after wetted out fabric has been layed in each side. 

here is what i picture working best, but i dont know exactly how to do it. 2 female mold halves and an air bladder to push the weave tight to the walls, but since im using sleeve, i need to be able to apply the sleeve layers to the bladder (partially inflated?) before laying it into one mold half, then bolt on other mold half, then inflate bladder.  im assuming this means i need to make a custom bladder that can be partially inflated that will be slightly smaller than the final size so it can be layed into the mold after weave has been applied and wetted out. i assume this type of bladder would also be made in a mold of its own, but needs to be smaller than the final mold. 

I have plenty of other questions about what to mill the molds out of and how to make custom bladders, etc. but i figured i should start by asking if i even have the right idea of how to tackle this, or if theres a better or easier way. any advice is greatly appreciated.  



Reply
quinn
q
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 155, Visits: 992
i think i might have an idea for how to make this happen. Theres a couple versions that all involve having a solid plug inside the bladder. i will have the 2 part female mold with seams top and bottom, an inner plug will be made that is smaller than the outer dimension of the boom by the thickness of the lay up plus maybe 2mm or so. The plug will be placed inside a regular bag type loose fitting bladder that will be vacuumed tight against the plug, then the layers of dry sleeve will be pulled over the plug/ vacuumed bladder and wetted out. this can then be easily placed inside the 2 part mold since it is a couple mm smaller in size. then vacuum is removed from bladder and air pressure applied which will expand the bladder that couple of mm pushing the sleeve layers tight to the walls of the 2 part mold. At this point the undersized plug will just be sitting inside the inflated bladder and its job is done. The only purpose of the male pug is to give a structure to brace the bladder into a slightly smaller than finished sized shape so lay up can be applied to it and wetted out. The question is, when inflating the bladder, is excess resin going to make its way to the ends of the mold and get pushed out? or just remain trapped inside?  
The other version works the same, except applying the dry sleeves to the vacuumed bladder/plug and leaving them dry while placing in the mold, remove vacuum, apply pressure, then set it up for vacuum infusion. for this to work the whole mold, with inflated bladder in it is then placed into a vacuum bag with air being pulled in one end and resin fed into the other end. This gets a bit tricky to get resin going where it needs to go. The vacuum bag would need to be sealed around both ends of the mold to prevent the resin from trying to pass around the mold instead of through it. probably also very tricky to get the resin to pull through the whole circumference instead of just part of it. This method may just not work at all. Pretty confident the first method would work, i just dont know how well the inflated bladder will push out excess resin. Probably the best approach is just to calculate the right amount of resin in the first place. Nice thing about this method is its relatively cheap. about 10 bucks worth of sleeve in each boom so i can afford to try a few times 
Edited 7 Years Ago by quinn
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
quinn - 7 Years Ago
Steve Broad - 7 Years Ago
quinn - 7 Years Ago
Steve Broad - 7 Years Ago
quinn - 7 Years Ago
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
oekmont - 7 Years Ago
Steve Broad - 7 Years Ago
quinn - 7 Years Ago
Hanaldo - 7 Years Ago
oekmont - 7 Years Ago
Steve Broad - 7 Years Ago
Fasta - 7 Years Ago
oekmont - 7 Years Ago
Steve Broad - 7 Years Ago
Steve Broad - 7 Years Ago
quinn - 7 Years Ago
Fasta - 7 Years Ago
quinn - 7 Years Ago
oekmont - 7 Years Ago
Fasta - 7 Years Ago
oekmont - 7 Years Ago
quinn - 7 Years Ago
Fasta - 7 Years Ago
quinn - 7 Years Ago
Fasta - 7 Years Ago
quinn - 7 Years Ago
Fasta - 7 Years Ago
quinn - 7 Years Ago
Fasta - 7 Years Ago
quinn - 7 Years Ago
Fasta - 7 Years Ago
quinn - 7 Years Ago
Fasta - 7 Years Ago
quinn - 7 Years Ago
Fasta - 7 Years Ago
Steve Broad - 7 Years Ago
quinn - 7 Years Ago
quinn - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search