Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
Yeh, a good point.
Ive been speaking to a friend of mine today who built his own CNC router with Chinese framework and American/German electronics. He uses it for cutting 10mm aluminium, mostly 2D/2.5D stuff but says he is sure it would do what I'm wanting it to do with ease. Extremely little backlash, doesnt get any chatter or lost steps so long as he keeps to 0.2mm passes and doesnt get impatient with the feeds, and he says it is accurate to 0.1mm as long as everything stays in tune.