I am in need of a consistent supplier for various types of Carbon Fiber Plate/Panels and was wondering if any of you had any feedback or suggestions?

I found this company online, their reviews look great as do their $prices$(From what I have searched for), but was wondering if any of you had used their products?

http://www.hillsidecomposites.com/standard-carbon-fiber-plate/#


Thanks
Replies
AeroSpaceOne
A
Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)
Group: Forum Members
Posts: 3, Visits: 21
Dean C - 6/7/2018 4:19:35 PM
Greetings,
For high quality Solid Carbon Fiber Sheets, Carbon Fiber sheets with Core, and custom work, check out dragonplate.com. We would be more than happy to serve your needs. Give us a call if you have any questions.
Best Regards,
Dean C
DragonPlate

Thanks, I have ordered from you in the past but am seeking a west coast supplier of carbon fiber products, mainly to cut down on shipping costs/times.
  I plan on ordering some of their Plate in a "Quasi Isotropic Weave"   http://www.hillsidecomposites.com/quasi-isotropic-carbon-fiber-plate/    
I will let you all know how it works out.
Thanks

Dean C
Dean C
Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)
Group: Forum Members
Posts: 5, Visits: 264
AeroSpaceOne - 6/7/2018 7:28:54 PM
Dean C - 6/7/2018 4:19:35 PM
Greetings,
For high quality Solid Carbon Fiber Sheets, Carbon Fiber sheets with Core, and custom work, check out dragonplate.com. We would be more than happy to serve your needs. Give us a call if you have any questions.
Best Regards,
Dean C
DragonPlate

Thanks, I have ordered from you in the past but am seeking a west coast supplier of carbon fiber products, mainly to cut down on shipping costs/times.
  I plan on ordering some of their Plate in a "Quasi Isotropic Weave"   http://www.hillsidecomposites.com/quasi-isotropic-carbon-fiber-plate/    
I will let you all know how it works out.
Thanks

Makes sense, good luck with your project!

AeroSpaceOne
A
Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)
Group: Forum Members
Posts: 3, Visits: 21
Dean C - 6/8/2018 8:57:51 PM
AeroSpaceOne - 6/7/2018 7:28:54 PM
Dean C - 6/7/2018 4:19:35 PM
Greetings,
For high quality Solid Carbon Fiber Sheets, Carbon Fiber sheets with Core, and custom work, check out dragonplate.com. We would be more than happy to serve your needs. Give us a call if you have any questions.
Best Regards,
Dean C
DragonPlate

Thanks, I have ordered from you in the past but am seeking a west coast supplier of carbon fiber products, mainly to cut down on shipping costs/times.
  I plan on ordering some of their Plate in a "Quasi Isotropic Weave"   http://www.hillsidecomposites.com/quasi-isotropic-carbon-fiber-plate/    
I will let you all know how it works out.
Thanks

Makes sense, good luck with your project!

Thanks,  I should be putting in an order for some tubing with you soon however.
Cheers

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search