I have a problem with my actual project. I am trying to copy the metal doorstep(?) of my car. The brand Name is pressed on it . I havedifferent imperfections between the letters but I have no idea to makethis better.I used xc110 210 Prepreg and tried to push everything down, but because thesign is overall about 10cm the space between the letters is pretty tight. So I do not think it was possible to press everything perfectly down. Next I used the xc110 450 and made a debulk. Then again a 210 and in the oven. Thevacuum of the bag was not perfect but I ran the pump all time so it should have been sufficient.I have seen that there was a topic about that, but after all I found no solution in the thread. Has someone a tip for me/practical knowledge how to solve that issue? Perhaps debulking after the first ply? Or lay very small snips of prepregs between the letters before laminating?
Thanks

Edited 7 Years Ago by SHaas
Reply
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Koenigs - 6/7/2018 10:02:26 AM

That was all basics of carbon fibers, but still pretty much best answer I've ever seen in internet.
Thanks for keeping up good and informative work, Matt!

Haha; thanks very much. We do our best Smile


Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search