Tolerance size of Carbon Fibre Square Box Section 20mm (17mm) - 1m Length


Tolerance size of Carbon Fibre Square Box Section 20mm (17mm) - 1m Length
Author
Message
frankideniso
f
Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)
Group: Forum Members
Posts: 5, Visits: 17
Hello,
From an older topic I know that the internal radii seems to vary between 3.6 and 3.8mm.  The outer radii varies between 4.8 and 5.2mm.  That has been measured by hand. Is this information still true today (any process improvement?). 
What about the tolerance of the 20 mm of the side of the tube ? Is it +/- 0.1 mm ? In my application the tube shall slide inside the groove of roller which looks like this one <https://www.aliexpress.com/item/10-56-31mm-belt-groove-H-type-injection-molding-machine-safety-door-roller-square-groove-D10/32816622292.html>. The groove profile shall fit the tube side profile as close as possible. 
Reply
oekmont
oekmont
Supreme Being (5.5K reputation)Supreme Being (5.5K reputation)Supreme Being (5.5K reputation)Supreme Being (5.5K reputation)Supreme Being (5.5K reputation)Supreme Being (5.5K reputation)Supreme Being (5.5K reputation)Supreme Being (5.5K reputation)Supreme Being (5.5K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
See you talking about the pultruded box section tubes? If you are thinking about some sort of structural mechanism I would advice against using them in that manner with roller support. Unidirectional tubes are really easily damaged when it comes to force transmission points. For very low loads it might work well.

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
frankideniso - 8 Years Ago
oekmont - 8 Years Ago
Warren (Staff) - 8 Years Ago
frankideniso - 8 Years Ago
oekmont - 8 Years Ago
frankideniso - 8 Years Ago
Dean C - 8 Years Ago
frankideniso - 8 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search