Author
Message
TURK
TURK
Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)
Group: Forum Members
Posts: 101, Visits: 662
Hi all,



I've got a few questions regarding the 'new' product 'XenCast Flexible Polyurethane Rubber' advertised on your website.

Basically I'm making a couple of moulds with the intention of casting 'Vac-Cast Epoxy Resin' into them,  what I need to end up with are two perfectly reproduced tooling plugs for vacuum forming my final parts into ABS plastic.



The following image will hopefully explain in greater detail my procedure.  I've recently used a product from 'Smooth-On' called 'OOMOO 30',  but had a disastrous result.  I must admit,  as good as it seems to be I just hate working with it.  Here's what my original mould box looks like with my plug secured in the base,  I then poured the silicon rubber into the mould box .........  it was an awful lot of work,  trying to mix what was a consistency of partly molten lava,  and the impossibility of pouring made the job needlessly difficult,  the result was a failed pour and a very badly formed mould  !  >>

 



Pouring the mix in a thin stream in a low corner was just impossible,  I almost had to resort to 'trowelling' it in ! >>

 



When I demoulded the following day,  it wasn't too bad,  but strictly speaking an appalling result.  Not something I would want to cast resin into that's for sure .........  I put it down to a good learning experience  >>





Because the silicon rubber wasn't 'fluid' enough,  full coverage of my plug wasn't achieved,  leaving large voids and air pockets  >>

 









So basically,  my question is,  would that 'XenCast flexible Polyurethane rubber'  be an alternative to OOMOO 30  ?

I've been looking at the 'XenCast PX30',  it seems to have the same characteristics as the OOMOO 30  ( both Shore A of 30 ),  how will it react to Vac-Cast Epoxy Resin being poured into it  ?







To further explain my situation my entire procedure is here >  Headlight mounting bracket moulds
Reply
TURK
TURK
Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)
Group: Forum Members
Posts: 101, Visits: 662
Hi Hanaldo,

Many thanks for your input,  very much appreciated mate  Wink

EC have an update version of that video? .............  looked everywhere,  can't find it   Sad

Matthieu Libeert' video on YouTube looks to be the best I can get my hands on right now >


The putty does look like great fun to work with  Smile  I take it it needs to be 'fibrous' like that, so it acts as a binding agent.

My plan,  as daft as it sounds,  is to apply the gelcoat ( very thick ) into this PETG headlight cover,  then add a centimetre or 2 ( preferably more ) of the putty.
It's the only way I can think of for creating a positive mould of the headlights with the two headlight apertures.  Once I have that I can continue onto the next stage,  making a tooling plug for vacuum forming the headlight covers in 3mm ABS.  Right now I'm just using two plastic containers to demonstrate where the headlight apertures will be  >>

A very crude mock-up of what I need to do,  using two plastic containers where the headlight units will be positioned  >>


My idea is to glue the cut down containers into the PETG plastic cover,  and work from the inside,  leaving me with a positive mould >>



I just need to familiarise myself with this moulding putty first,  to see of this method will work.  The only concern I have right now is,  will the tooling gelcoat stick to the PETG plastic?   
I know this method will never give me a structure ( mould ) strong enough for vacuum forming,  I'm only interested in the actual form right now.  Once I have those I'm pretty sure I can make another mould to create some vacuum forming tooling plugs using Vac-Cast Epoxy Resin.

Oh,  almost forgot! ..................  many thanks to Matthieu for the YouTube video  Wink


TURK


Edited 8 Years Ago by TURK
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
TURK - 9 Years Ago
Hanaldo - 9 Years Ago
TURK - 9 Years Ago
TURK - 9 Years Ago
Hanaldo - 9 Years Ago
TURK - 9 Years Ago
Warren (Staff) - 9 Years Ago
TURK - 9 Years Ago
Warren (Staff) - 9 Years Ago
TURK - 9 Years Ago
nc42 - 9 Years Ago
TURK - 9 Years Ago
Rich (Staff) - 9 Years Ago
TURK - 9 Years Ago
Rich (Staff) - 9 Years Ago
TURK - 9 Years Ago
Rich (Staff) - 9 Years Ago
TURK - 9 Years Ago
TURK - 9 Years Ago
Hanaldo - 9 Years Ago
TURK - 9 Years Ago
Hanaldo - 9 Years Ago
TURK - 9 Years Ago
Warren (Staff) - 9 Years Ago
TURK - 9 Years Ago
TURK - 9 Years Ago
TURK - 9 Years Ago
Hanaldo - 9 Years Ago
Warren (Staff) - 9 Years Ago
TURK - 9 Years Ago
Warren (Staff) - 9 Years Ago
Rich (Staff) - 9 Years Ago
Hanaldo - 9 Years Ago
TURK - 9 Years Ago
TURK - 9 Years Ago
TURK - 9 Years Ago
TURK - 9 Years Ago
TURK - 8 Years Ago
Hanaldo - 8 Years Ago
TURK - 8 Years Ago
Hanaldo - 8 Years Ago
TURK - 8 Years Ago
Hanaldo - 8 Years Ago
TURK - 8 Years Ago
Hanaldo - 8 Years Ago
TURK - 8 Years Ago
Hanaldo - 8 Years Ago
TURK - 8 Years Ago