Finishing Surface of Foam Pattern


Author
Message
jamesw
jamesw
Supreme Being (715 reputation)Supreme Being (715 reputation)Supreme Being (715 reputation)Supreme Being (715 reputation)Supreme Being (715 reputation)Supreme Being (715 reputation)Supreme Being (715 reputation)Supreme Being (715 reputation)Supreme Being (715 reputation)
Group: Forum Members
Posts: 61, Visits: 558
I'm working on some CNC cut foam patterns, and after some advise on which products/methods to use to get a suitably surfaced pattern for taking the mould...

The surface isn't perfectly smooth, with many small pockets from the machining process - see attached image (slightly worse in places)

My original plan - (and have ordered these bits) was to use your epoxy coating resin with glass bead & silica and then brush/spray onto the surface - do you think that will be sandable to a suitable surface finish? should I be looking at adding some 163g woven glass over the part? These are largish parts for car bodywork...

Many Thanks,
James
Attachments
20120608_120833.jpg (814 views, 248.00 KB)
Replies
jamesw
jamesw
Supreme Being (715 reputation)Supreme Being (715 reputation)Supreme Being (715 reputation)Supreme Being (715 reputation)Supreme Being (715 reputation)Supreme Being (715 reputation)Supreme Being (715 reputation)Supreme Being (715 reputation)Supreme Being (715 reputation)
Group: Forum Members
Posts: 61, Visits: 558
One other question,

Would you still use the epoxy coating resin for skinning with 163g - or something else?

James
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi James,

Yes, the Epoxy Coating Resin is perfect for pattern finishing. I'd say it's the best of our resins for this application. You can mix in some microballoons as well, if you wanted to make it more sandable.

--Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
jamesw - 14 Years Ago
Matt (Staff) - 14 Years Ago
jamesw - 14 Years Ago
Matt (Staff) - 14 Years Ago
jamesw - 14 Years Ago
jamesw - 14 Years Ago
Matt (Staff) - 14 Years Ago
jamesw - 14 Years Ago
Matt (Staff) - 14 Years Ago
jamesw - 14 Years Ago
jamesw - 14 Years Ago
Matt (Staff) - 14 Years Ago
jamesw - 14 Years Ago
Matt (Staff) - 14 Years Ago
jamesw - 14 Years Ago
Matt (Staff) - 14 Years Ago
jamesw - 14 Years Ago
jamesw - 14 Years Ago
Matt (Staff) - 14 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search