EL2 resin seemingly not curing / cracked looking and tacky days later.


EL2 resin seemingly not curing / cracked looking and tacky days later.
Author
Message
jprovan3141
j
Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)
Group: Forum Members
Posts: 2, Visits: 5
I've noticed on a few test pieces i have created that the face touching the mould / surface is lovely smooth, flat, perfectly cured, however the face open to the air is still tacky especially when in contact with sweat from hands / slight dampness in any way.

I'm quite confident i've got the ratios correct, i've used two separate scales, the second more accurate than the first, and mixed thoroughly - i mix in a mixing pot with a wooden spatula for 3+ mins or so, yet it still comes out this tacky / cracked looking way. 

I have tried post-curing the piece in an oven, however this hasnt got rid of the tackiness and has exacerbated the "cracked" look. See attached picture for the piece from the oven, however i assure this is how my other pieces have looked also, just less-so.

Could anyone give me some advice on where i'm going wrong ? I've done enough playing and want to start seriously making some working prototypes but i cant seem to work out what the problem is here. In the attached photo i was hoping for that nice, shiney, stereotypical carbon fibre look but uhh....not so...  

Thanks, J.
Attachments
IMG_20180410_175129.jpg (530 views, 1.00 MB)
IMG_20180410_175139.jpg (468 views, 1.00 MB)