Group: Forum Members
Posts: 550,
Visits: 27K
|
Why do you need such a failure line? I can't really think of a reason this would improve safety. such a pure carbon failure line might snap in a crash, but leaving half a bonnet flying through the air, wich can't be your goal. the soric core improves the splintering characteristics over a pure carbon structure. and a soric core with just a single layer carbon on either side will imply less forces on the crash object than a regular steel bonnet any way.
however, 2 layers of 200g carbon will be extremely flexy without a curved surface. so if this is the bonnet you are planning to do, this will likely make a wobbly bonnet. additionally you will see the corner of the soric core through the top layer, resulting in two lines across the bonnet.
If you really want crash safety, I would recommend getting some lightweight Kevlar, an add it below the surface layer, above the soric. cut it a few cm smaller than the bonnet, because Kevlar really doesn't leave nice post cure cutting edges. if you want to stick to your plan, reduce the soric thickness in the failure zone. for example from 3mm to 2mm. this will leave enough stiffness, but will create a weak line.
|