Hello friends,
I intend to make a medium-sized piece (1.35mx 0.30m) with polyester resin, but I saw that it corrodes the potential risk of shrinkage during resin curing.
- The resin has the gel time of: 30 minutes and the manufacturing process would be by Hand Layup + vacuum bag or Resin nfusion.
The doubts are as follows:
"What do I have to do to stop this from slowing down?" Because I can not have dimensional changes due to the product accessories.
Desmoulding after 4 hours of lamination cause me problems?
We have a small production line and we need to be quick in our process.
Thanks, Dezer
|