Hi,
I just tried to make a mould using the Unimould System, and was a bit surprised by the smell of the gel coat Smile

Are there any other ways to make a mould but not evaporating so much unhealthy stuff?

Can this work?
1) Doing the moulds based on resin infusion out of glass or carbon fibres?
2) Epoxy Mould Making system? maybe it does not smell...

Of course I use the mask and the room is ventilated, nevertheless its still very smelly....

Thank you in advance for the answer
Reply
CMax
C
Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)
Group: Forum Members
Posts: 9, Visits: 38
Thank you Warren,
1 more question with regards to the mould making based on resin. I will then use EG60 Epoxy Tooling Gelcoat. What should be the process if I want to use the woven glass on top? Few sentenced would be enogh, thank you in advance
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
CMax - 7 Years Ago
Hanaldo - 7 Years Ago
Warren (Staff) - 7 Years Ago
CMax - 7 Years Ago
Warren (Staff) - 7 Years Ago
CMax - 7 Years Ago
Warren (Staff) - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search