+x oekmont - 1/30/2018 7:07:42 PMthe flexibility highly depends on the wall thickess and the fibre orientation. if you are looking for carbon fibre, a tube with the fibres at +-45° would be the most flexible. it should be no problem to make a laminate, that may clip over the slightly bigger diameter, and still sits quite strong.however, glass fibres got better absolute elastic propertys. they are able to flex more without breaking.