	Group: Forum Members 	        
    Posts: 36, 
    Visits: 65 
    
 
          
		     | 
				                       
                 
                
                    
			            Thanks Warren...in which case, part two of question :-).
  I mixed some glasscast for the first time on Sunday...fresh tin;, never opened, only a month or two since ordered.
  I made up 60g, so 40g resin, 20g hardener. Few drops or your red translucent pigment. Stirred it well by hand, cast it into a silicone mould made two days before.
  How hard should the product be after two days? It still has a distinct “taffyish” feel...it’s only a 100x100 square by 4mm deep.