TechnoStuck
T
TechnoStuck
posted 7 Years Ago
ANSWER
HOT
Topic Details
T
Group: Forum Members
Posts: 1,
Visits: 6
I have never tried anything like this before. My project is, I have an perspex desktop which has a crack in it and has started to craze in places. So I thought I would cover it with epoxy resin. So I joined this forum for help with this project
Reply
Like
2
Warren (Staff)
Warren (Staff)
posted 7 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
Welcome to the forum! It should be possible to coat it with an
Epoxy Coating Resin
such as our GlassCast which can be coated up to 15mm thick per layer. That might give you the look you are after.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search