Got it from my local composites supply store. Its just generic GP330, very common stuff. 
asmasm
asmasm
Supreme Being (159 reputation)Supreme Being (159 reputation)Supreme Being (159 reputation)Supreme Being (159 reputation)Supreme Being (159 reputation)Supreme Being (159 reputation)Supreme Being (159 reputation)Supreme Being (159 reputation)Supreme Being (159 reputation)
Group: Forum Members
Posts: 15, Visits: 189
I read most of the thread but didn't see this mentioned. What resin system are you using? Any post cure?
Hanaldo
Hanaldo
Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
I'm using Renlam K3600, or Araldite LY K3600 (the names seem to be interchangeable). Simple post cure of 80 degrees for 4 hours brings the Tg up to 93 degrees C. 
Jadleybray
Jadleybray
Supreme Being (210 reputation)Supreme Being (210 reputation)Supreme Being (210 reputation)Supreme Being (210 reputation)Supreme Being (210 reputation)Supreme Being (210 reputation)Supreme Being (210 reputation)Supreme Being (210 reputation)Supreme Being (210 reputation)
Group: Forum Members
Posts: 10, Visits: 85
Great read, bummer pictures lost.  