Group: Forum Members
Posts: 13,
Visits: 70
|
Yeah I would like to know too, because I sometimes spray the resin with pistol, and its hard to clear it. The same is with brush, I cannot clean it with acethone, when brush is wet with acethone its ok but after it dryies the brush become useless... How you hanlde with this silly problem ?
|