Complete Introduction to Prepreg Carbon Fibre (Using our new XPREG XC110 system)


Complete Introduction to Prepreg Carbon Fibre (Using our new XPREG XC110 system)
Author
Message
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
I've just published our latest video tutorial. This is the third and final part of the latest series which now covers the making of a carbon fibre engine cover from CAD model to prepreg carbon fibre part.



In this final video we're using our new XC110 prepreg which replaces the Easy-Preg that we've used and sold for many years. The decision to move away from the Easy-Preg system was a very big one and is something that we've been working towards for a very long time. Easy-Preg worked fantastically and was a great product but there were a number of drawbacks which we hope to have overcome with the new XC110 system. Namely, these were that the Easy-Preg system was limited to a specific surface ply (a 240g 3k) which could not be substituted for any other weight or weave (so finely balanced was a the behaviour of the material) and, to be perfectly honest, the very high price of the material (owing to the difficult manufacturing process).

Therefore, we hope to have achieved a number of things with the new XC110 prepreg:

Firstly, we now have a range of out-of-autoclave materials, including a 3k 210g, a 12k 450g (both of which could be used as the surface ply), as well as compatible unidirectional (UD) material and  an adhesive film. Having such a comprehensive offering means that even the most complex structural projects can be undertaken 'out-of-autoclave'. 

Secondly, by controlling the production of these materials from creel-set to freezer we have been able to significantly reduce the price of these materials so that they now compete with just about any prepreg system, let alone a high performance out-of-autoclave system. Of course, due to the extra admin and overheads of handling prepregs there is still quite a bit extra to pay on very short rolls (1m, 2m etc.) but, as an indication, a 25m roll of either the surface or backing is available from us at around £30 (34 euro, $40 usd) with further discounts available for larger orders. Download our full prepreg price list here.

There are however some significant differences between the Easy-Preg system and the new XC110 system so I thought this topic might be a good place to discuss them and take any questions people have. The most significant differences are:
  1. XC110 is far more sensitive on the cure cycle. To get good results it's really important to follow a two-stage post cure with carefully controlled temperature. Full details of the recommended cure cycle can be found in the XC110 Out-of-Autoclave Complete Processing Guide PDF.
  2. XC110 doesn't really seem to like vinylester mould surfaces (such as Uni-Mould). Obviously this is a huge disappointment to us because we have previously stated that Uni-Mould moulds can be used to for relatively low curing of prepregs. Although - at a push - the XC110 system can be cured in a vinylester mould it does seem to increase the chances of surface imperfections (pin holes) due to a combination of reaction with the vinylester and the fact that the preferred cure cycle for the XC110 (which finishes at 120'C) cannot be used because the Uni-Mould tools cannot take this temperature. Therefore we now suggest moulds made using either epoxy tooling prepreg or moulds made using high temperature epoxy gelcoat backed up with either high temp epoxy paste or high temp epoxy resin.
  3. Bagging method: Better results are achieved with this prepreg system by not putting breather on the back of the release film where it is over the laminate (as can be seen in this video).
I hope you enjoy the new tutorial and would be happy to answer any questions anyone may have on this new system.


Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Reply
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hanaldo - 12/11/2017 12:33:15 AM
I have been doing a bit of experimenting with the XC110 in the last couple of weeks, so I'll do a little 'first impressions' write up along with some pictures later today. 

Nice one Martin, it will be interesting to hear your feedback (as you have experience of both materials). I'll be totally honest and say that we have had a few teething problems with customers who are familiar with the Easy-Preg not getting great results at first with the XC110. The main reason seems to be the difference in the way they need to be processed, if you just try to swap one for another and process in the same way then it won't work, but once we've been able to work with customers, explain the differences and iron out any problems the feedback seems to be good. In one case we even got a customer to send a mould they were struggling with to us so that we could demonstrate laying it up and making it correctly - we made a video of the whole process and shared it with the customer which then gave them the confidence that it really does work the way it should. They are now creating great parts and are very happy.


Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Matt (Staff) - 9 Years Ago
Hanaldo - 9 Years Ago
Matt (Staff) - 9 Years Ago
cumberdale - 9 Years Ago
Matt (Staff) - 9 Years Ago
Hanaldo - 9 Years Ago
cumberdale - 8 Years Ago
Hanaldo - 8 Years Ago
Steve Baker - 8 Years Ago
kip - 8 Years Ago
Hanaldo - 8 Years Ago
kip - 8 Years Ago
Hanaldo - 8 Years Ago
             Any pictures yet ?
kip - 8 Years Ago
Hanaldo - 8 Years Ago
Hanaldo - 8 Years Ago
Thomb - 8 Years Ago
kip - 8 Years Ago
Hanaldo - 8 Years Ago
kip - 8 Years Ago
Hanaldo - 8 Years Ago
FRTCARBON - 7 Years Ago
FRTCARBON - 7 Years Ago
     nice
FRTCARBON - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search