Additives to create light-diffusing properties in cast resins?


Author
Message
Ren Delf
Ren Delf
Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)
Group: Forum Members
Posts: 2, Visits: 34
Hello folks. 

I'm fairly new to the composites game, having only really used epoxies to create glassy finishes on work surfaces so far. 

I'm currently making some prototypes, and want to create a piece of cast resin which will diffuse light similarly to commercially available polycarbonate diffusing sheets. 

I'm hoping to use standard casting resin, a silicon mould/other form and an additive. 
I've read that there are silicon-based products that may be able to achieve this effect, but haven't been able to ascertain if this is the case or what I'd need to use. 

Any help appreciated! 

Cheers, 

Ren 


Edited 9 Years Ago by Warren (Staff)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search