It says in the technical datasheet of Easy Composistes out-of-autoclave Prepreg XPREG XC110, that for curing the "minimum vacuum pressure is 10mbar". This is a pretty low value. There are many vacuum pumps that can only achieve 50mbar, for example.

So my question basically is: why so low? To reduce the probability for pinholes? Because the relative gain in pressure when going from a 50mbar vacuum pump to a 10mbar vacuum pump is very small when you compare it to the outside pressure of a thousand mbar (well: 960mbar where I live).
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
The 10mbar figure is based on sea level and standard atmospheric pressure ie 1 bar/1000mbar, so the higher you go, the less force is applied against the bag, so realistically with a very high vacuum pump, for exmple 0.03mbar, then as you approach 900meters or 900mbar atmospheric (eg a lower altitude in a severe "low pressure" weather storm), then the level of force applied to the vacuum bag and hence the pre-preg may well not be enough to ensure a pin hole free finish without extra force being applied, such as in a press or an autoclave.

However this is quite a rare scenario for most users.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
cumberdale - 8 Years Ago
Warren (Staff) - 8 Years Ago
cumberdale - 8 Years Ago
Warren (Staff) - 8 Years Ago
cumberdale - 8 Years Ago
Warren (Staff) - 8 Years Ago
cumberdale - 8 Years Ago
Warren (Staff) - 8 Years Ago
     Thanks. :)
cumberdale - 8 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search