Clear Coat Disaster...


Author
Message
fibernoob
fibernoob
Supreme Being (662 reputation)Supreme Being (662 reputation)Supreme Being (662 reputation)Supreme Being (662 reputation)Supreme Being (662 reputation)Supreme Being (662 reputation)Supreme Being (662 reputation)Supreme Being (662 reputation)Supreme Being (662 reputation)
Group: Forum Members
Posts: 34, Visits: 134
Sure ... it also didn’t add up.

I changed the clear as a last resort since I had redone all the rest.



Before applying to the carbon we tested on metal and interestingly enough the one that least stuck do the carbon had a better result on metal and vice-Versa.

On pure resin (left over from infusion) both stuck perfectly. So I then blamed the release agent.

To make sure ..... I made a quick sheet and added both wax based and pvc release agent to test.(possible release agent in the fiber opening clear)


The newer clear seemed to perform better again.

My only guess would be possible better chemical compatibility between them ...


Thanks for the reply ... I will keep testing.