Hi,

I have a question regarding curing epoxy to get the best results. The project is a hand layup of fiberglass 3 oz and I'm working with a room temperature curing epoxy with the following properties:
- Gel Time (@ 21C) 38 min
- Demold Time 24hr
- Deflection temp 53 C
- full cure at room temperature 7 days

I'm a lite confused about what is considered the
"
curing'' and 
"post-cure" period, when and how much heat to apply (and for how long).


Thanks

Alexandre

Alexandre
A
Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)
Group: Forum Members
Posts: 4, Visits: 11
Alexandre - 11/2/2017 1:21:33 PM
Hi,

I have a question regarding curing epoxy to get the best results. The project is a hand layup of fiberglass 3 oz and I'm working with a room temperature curing epoxy with the following properties:
- Gel Time (@ 21C) 38 min
- Demold Time 24hr
- Deflection temp 53 C
- full cure at room temperature 7 days

I'm a lite confused about what is considered the
"
curing'' and 
"post-cure" period, when and how much heat to apply (and for how long).


Thanks

Alexandre

Oh and how the heating affect the full cure time?

Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
The demould time is when you can remove it from the mould.  The epoxy will only be partially cured at demould and depending on temperature, can take a few weeks to a month or two to fully cure internally.

A post cure is used to either accelerate the cure process and/or to maximise the HDT  of the resin by  doing an additional higher temperature cure after the main cure at room temperature..

The manufacturers data should list the  recommend post cure cycles and if you can cure the resin at elevated temperature from the outset.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Alexandre
A
Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)
Group: Forum Members
Posts: 4, Visits: 11
Thanks for the quick answer!

So main cure and post-cure should be specified by the manufacturer?  In my case there doesn't seem to have this information, can anything be done in this case?

Alexandre
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Alexandre - 11/2/2017 1:44:26 PM
Thanks for the quick answer!

So main cure and post-cure should be specified by the manufacturer?  In my case there doesn't seem to have this information, can anything be done in this case?

Alexandre


I would definitely email the manufacturer. If they have no data on even the simplest room temperature cure times then I would probably consider then fairly incompetent! 


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Not uncommon to find no post-cure data, but generally you should always be able to find a 'Tg' or 'HDT' value, which is the upper temperature limits of the resin. For most entry level epoxies this is around 60 degrees.

If you can't find any data at all, I would hazard a guess at it being around a 60 degree Tg, so you could do a post-cure of 60 degrees for 16 hours. Ideally you would ramp up to this temperature slowly, 0.5-1 degree per minute. 
Alexandre
A
Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)
Group: Forum Members
Posts: 4, Visits: 11
I've gotten word from the manufacturer and indeed the epoxy is not designed for high temperature applications.
Hence, they don't suggest any curing schedule.