Hi guys after some advice. I'm using all easy composites vac bag supply and pump.
I'm having major issues with bag leaks,  with the pump on its perfect but dosnt hold it once it's off,  and I'm not leaving the pump on for 2 hours lol.
Any way of checking and finding where the leaks are with any device. ? 
Also do you have to seal the hose onto the push connectors or will they be ok and airtight. ? 
Iv even tryed a flat bag and still leaks.. :s
I'm going to order the vac gauge,  anything other help would be grear lol..

Cheers
Reply
Finnluxury
Finnluxury
Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)
Group: Forum Members
Posts: 50, Visits: 448
Buy a Micron meter. It will stop all your problems. basic vacuum gauge is too inaccurate. With Micron meter u can see live feed of the possible leaking. I only start infusing after I get vacuum of under 980microns. When typical vacuum gauge shows you a perfect vacuum, then micron meters just starting to life (shows 150.000microns). Then i run pump till I get it to 980 microns. When I bought this part, I never had any problems anymore. U cant hear tiny leaks even using the ultrasonic device. 

This is cheap versio and works like a dream:
https://www.trutechtools.com/BluVacMicro
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Interloper393 - 8 Years Ago
MarkMK - 8 Years Ago
scottracing - 8 Years Ago
Warren (Staff) - 8 Years Ago
rmaddock - 8 Years Ago
Interloper393 - 8 Years Ago
Warren (Staff) - 8 Years Ago
MarkMK - 8 Years Ago
Interloper393 - 8 Years Ago
Finnluxury - 8 Years Ago
MarkMK - 8 Years Ago
Interloper393 - 8 Years Ago
Finnluxury - 8 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search