GlassCast Epoxy Surface resin - multiple pours!


Author
Message
Copieg
Copieg
Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)
Group: Forum Members
Posts: 5, Visits: 48
Hi,

I've bought the clear cast epoxy resin for a "valley" table top I'm making. The total thickness will be approximately 28mm. The resin will only do 15mm in one pour. How do I go about doing the 2nd pour? Do I have to wait until it's full cured (several days??!) will the surface need sanding (keyed) before I pour the 2nd layer?


Also, I will need to sand the resin once fully cured, because the want the wood either side of the resin to be visible (not covered in resin) so will I need to go through all the grits 120-1500 wet dry and then use a cutting compound to polish it?


Any help will be greatly appreciated!

Thank you.


Edited 8 Years Ago by Warren (Staff)
Replies
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Its hard to tell from the picture but are the bubbles in the surface coat or the sealing coat?  It could be the sealing coat had some voids in that opened up with sanding and now show up. It's not something we have seen like that before.  How humid is the environment?  Excessive moisture can cause a reaction similar.

Recovery would involve sanding it right back and starting afresh..



Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Copieg
Copieg
Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)
Group: Forum Members
Posts: 5, Visits: 48
The bubble are in the main coat, not the sealant coat. The seal coat was perfect.

I don't know if there was too much moisture in the air, I have now way of testing that. Sad