Problem: Soft and Flexble CF parts ...


Author
Message
fibernoob
fibernoob
Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)
Group: Forum Members
Posts: 34, Visits: 134
Hi All, 

I have tried to find some info on here but possibly did not use the same search terms so please excuse me if this has been repeated.

I have made some CF panels on a glass sheet  using 2 x 200gm² sheets pressed together. In one case i have used peel ply on the reverse to clear excess resin.


I have noted that these parts and panel came out soft and flexible.  It also has a slight wrinkled surface when folded or flexed.

The flexibility can be compared to that of a common computer mousepad.



Anyone had this happen or have an explanation ?


The only reason I can possible think of is ambient temperature, I remember the days where pretty cold and humid during and my workshop is an open space.

I have also let the parts rest for a few says hoping that they would cure and harden a little... but no luck.

Seems like this panel and other parts I made during those days have all come out the same way...   Blink

http://www.talkcomposites.com/Uploads/Images/ede72a04-6225-42a7-8273-54e6.JPG 
Reply
fibernoob
fibernoob
Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)
Group: Forum Members
Posts: 34, Visits: 134
Hey all....  After reading the replies, remembering what happened and calling the suppliers ... I found out what went wrong w00t

I had purchased  lower viscosity resin thinking that it would produce less air bubbles during the vacuum process.

ExclamationIt occurs that this resin has a slightly different mixing ratio and is more sensitive to temperature. Exclamation


Thanks again for all the helpful input from everyone, nice to see how accurate all the answers are.