Matthieu Libeert
Matthieu Libeert
posted 8 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
Hi everyone! I'm launching a new series of videos.
Like I've mentioned in the video I learned to infuse thanks to the videos of Easy Composites
Thanks again for that video! changed my life!
I'll be working on more of these videos where I "talk" a bit more
If you have some suggestions for coming video's please write them down below!
Matthieu
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search