I mostly use EasyLease in my moulds, and usually they do not need very much "cleaning" as such .. I polish them with a clean cloth, and put on a few new coats of Easylease.
If I need to go from wax release to Easylease, I clean the mould very thoroughly with Alcohol, acetone and EC Mould Cleaner, then apply at least 6 coats of Easylease .
If I need to polish up a mould, I clean with Acetone and then polish .. then as above ..