Author
Message
Coxo
Coxo
Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)
Group: Forum Members
Posts: 39, Visits: 476
dose any one no if you can thin down duratec 
For spraying ? 
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
The duractec data sheets say to use MEK.




Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yep, use pure MEK (which is all the Duratec thinners is). 

You can use acetone, but in my opinion it doesn't work well - flashes too quick, so you get lots of dry over spray and orange peely areas. 
Coxo
Coxo
Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)
Group: Forum Members
Posts: 39, Visits: 476
Thanks guys 
Coxo
Coxo
Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)
Group: Forum Members
Posts: 39, Visits: 476
How much should I put in when mixing like say 
100grams 
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
Coxo (08/05/2017)
How much should I put in when mixing like say 
100grams 


Coxo
Coxo
Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)
Group: Forum Members
Posts: 39, Visits: 476
Thanks 
Coxo
Coxo
Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)
Group: Forum Members
Posts: 39, Visits: 476
Where did u get it from fasta  I tried kirkside 
But they don't sell it 
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Gotta get it from ATL in Queensland mate, they are the only distributors of it in Australia now. 
Coxo
Coxo
Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)
Group: Forum Members
Posts: 39, Visits: 476
I got some from fibre glass resin  supply's In  Welshpool 
GO