Hey Kirk ,

I would agree with what Davro says.

I tried skinning and even small parts can take 2 weeks to perfect. Like i did my ignition barrel and even that has a fitting issue so doing panel edges would cause a lot of issues and if you want it as a demo car would you really want scuffed carbon etc?

If you are starting carbon parts / skinning as a company service you better have a lot of time and patience and the best of conditions for letting the epoxy cure.

any moisture in your garage will ruin the coat i have first hand experience with this and it's devastating.

You say about wanting to do skinning instead of infusion and prepreg because of cost but skinning parts will never be as good quality and infusion/prepreg and if i was running a business quality is everything.

If you did get into making molds you can get into pattern making and then your demo car could have custom made body parts exclusive to that car and your company.

I will be doing a full carbon makeover of my car when i have the time away from work and ill be doing it with infusion.
Coxo
Coxo
Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)
Group: Forum Members
Posts: 39, Visits: 476
Hi fasta will u be a your unit tomorrow 
And I'll pop in ? 

 Cheers graham 
Fasta
Fasta
Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
I'll be there first thing in the morning hour or so from 9am.

40 deg C public holiday, too hot for work.




Edited 9 Years Ago by Fasta
Coxo
Coxo
Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)
Group: Forum Members
Posts: 39, Visits: 476
Cool see u at 9 am  I forget it's a holiday 
Coxo
Coxo
Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)
Group: Forum Members
Posts: 39, Visits: 476
That duratec tec sun sheid is great  look at the finish 
Thanks fasta for giving me some to try 
How long dose it take to dry   It still seams 
Tacky  but hard if u no what I mean 
Attachments
IMG_4659.JPG (290 views, 541.00 KB)
Fasta
Fasta
Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
Assuming the catalyst was the right one then it should be ok overnight to sand. 




Coxo
Coxo
Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)
Group: Forum Members
Posts: 39, Visits: 476
Just the mekp  one I used from kirkside 
Is that the right one   Fasta. 
Hanaldo
Hanaldo
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
The MEKP from Kirkside will work fine mate. 
Coxo
Coxo
Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)
Group: Forum Members
Posts: 39, Visits: 476
Yes it dryed and jeso it's easy to flatten back. great product 
 Has any one tryed kbs Dimond clear coat 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search