Is Carbon fibre rod suitble for making marine dan buoy?


Author
Message
Fram
Fram
Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)
Group: Forum Members
Posts: 2, Visits: 9
I am thinking of using a 2m length of 5mm rod to make a marine danbuoy which I will use as a pick up buoy on a swinging mooring for my 30ft boat. This rod will pass through a float and have a weight attached to the base to keep it upright. Do you think that carbon fibre would be a suitable product for this purpose please and, if so, would a 5mm rod be appropriate or should it be a larger diameter?  Many thanks, Colin 
Reply
Fram
Fram
Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)
Group: Forum Members
Posts: 2, Visits: 9
Thank for your replies, Warren and Dravis, much appreciated.

Colin