Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
skinning / plastic
skinning / plastic
Post Reply
Like
8
skinning / plastic
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
easby
easby
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 6,
Visits: 44
Hi, this may of been talked about but not come across it yet so easier to ask.
What do you guys recommend or do to make sure carbon does not delaminate from plastic ie bumpers?
I have read a lot about making sure surface has a good key and using blade to put deep cuts in etc but just thought I would ask someone may have other ideas I have not seen yet. Thanks Andy
Tags
bumper
laminate
plastic
resin
skinning
Reply
Like
8
Matt (Staff)
Matt (Staff)
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 680,
Visits: 1.9K
Hi Andy,
It really depends on the type of plastic you're bonding to. The bond of epoxy to ABS can be improved by flame-treating the ABS. I'd recommend running some trials through because often no much prep is necessary to result in a good bond. However, there are some *really* difficult to bond to plastics which epoxy simply won't touch (think polypropylene, polyethylene) which would either need some very specialist priming or to be avoided altogether.
Most plastic car trim parts I've seen recently actually say what plastic they're made from as part of the markings on the injection moulding.
I hope this helps,
Matt
Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Tags
ABS
bumper
delamination
plastic
skinning
Reply
Like
7
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
8
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search