Hi all,



I'm in need of a little help guys  ........  I watched ( and learned a great deal ) from Paul's 'Airbox' video on YouTube,  I purchased and currently using the Low Density 48Kgs/m3 PU foam blocks, to get my 'form'.  I then put a skim of body filler to harden the 'form' that will eventually be my plug for casting a resin mould.  After the initial body filler 'skim' had hardened,  I applied a few more layers of body filler to build-up the form to the dimensions I wanted.  So basically,  my plug now has about 3mm of body filler on it that needs to be sanded down smooth.

Unfortunately,  that isn't what happened ...........  the body filler ( known as 'Bonda' ) turned out to be more like a rubbery texture !!!  Crazy    as we all probably know,  it's impossible to sand down bubble gum !

Any of you know why it did this ? ..........  did I overdo the 'skimming' of body filler ?

The plugs have now been drying for four days,  but the texture of the body filler is still quite soft, to the point where I can push my finger nail into it.

This was the original 'skim' of body filler   >>

 



Then I applied a little more on  to build it up as it were,  so I could sand down the contours   >>

 





So,  another question if I may .........  As I've never had any troubles with this sort of body filler,  I use it all the time ( mostly on MDF plugs ) and never had any issues with it.  D'you think there's been kind of a reaction with the PU foam ?  should I have applied a few layers of Pattern-Coat Primer to the initial 'skim' of body filler ?  or can I simply apply Pattern-Coat Primer directly onto the PU foam ?  ( sorry, that's three questions ! )



There's loads more info in the following link,  and the entire procedure  here >  PU foam plugs




Many thanks for your time.






TURK
Edited 9 Years Ago by TURK
Reply
TURK
TURK
Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)
Group: Forum Members
Posts: 101, Visits: 662
Thanks chaps,  makes a great deal of sense that  BigGrin

I tried to fix my previous plugs, but I think I was flogging a dead horse  !  Sad   So I started again.



The nice people at 'Easy Composites' kindly sent me some more PU foam ..........  I'm in a tiny village in central France,  but it's not a problem for them ..........  I had to pay for it thought !    BigGrin



I'm now using the slightly denser PU foam,  96Kg/m3.  You could say it has the consistency of Balsa wood,  great to work with.  The final shape I'm trying to achieve is quite intricate,  in order to have a vacuum forming friendly shape I can't have any negative angles,  straight vertical side walls are also an issue,  but I really need that 'footing' it's part of the area that will be bonded to the headlight retainer  >>

 


And as advised,  I applied the Pattern-Coat Primer directly to the PU foam .........  it's worked very well indeed.  When that cures I'll sandback and fill any gaps and low spots with body filler, then a final Pattern-Coat Primer application  >>

 




I'll let you know what happens .........





Many thanks all for your help and advice guys.









TURK
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
TURK - 9 Years Ago
FLD - 9 Years Ago
Warren (Staff) - 9 Years Ago
TURK - 9 Years Ago
Warren (Staff) - 9 Years Ago
Hanaldo - 9 Years Ago
TURK - 9 Years Ago
Hanaldo - 9 Years Ago
Dravis - 9 Years Ago
TURK - 9 Years Ago
Hanaldo - 9 Years Ago
TURK - 9 Years Ago
Warren (Staff) - 9 Years Ago
TURK - 9 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search