Hanaldo (30/11/2016)
Don't apply chemical release agent over the top of wax!!! It's ok to add wax on top of a solvent based release agent, but you can't put a solvent release agent on top of wax, it will dissolve the wax and contaminate the underlying release agent. 

With any lucky you might get away with it, but just for future knowledge! It's always always at least 4 coats of chemical release agent, and then you can do a couple coats of wax on top of that to increase the surface tension then you can do that, buy remember to buff as light as possible, don't buff off your release agent. 


Thanks Mate 

ill do that from now on 
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Don't apply chemical release agent over the top of wax!!! It's ok to add wax on top of a solvent based release agent, but you can't put a solvent release agent on top of wax, it will dissolve the wax and contaminate the underlying release agent. 

With any lucky you might get away with it, but just for future knowledge! It's always always at least 4 coats of chemical release agent, and then you can do a couple coats of wax on top of that to increase the surface tension then you can do that, buy remember to buff as light as possible, don't buff off your release agent. 
MiggzFSU
MiggzFSU
Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)
Group: Forum Members
Posts: 7, Visits: 50
thanks for the feedback guys 

iv corrected the voids and bridging as well as i could, that last pic was only 1 layer light strand and 1 layer of the heavier one, iv added 2 more layers of the heavier since the pic was taken . 

Sorry about the quality of this mold its my first attempt at this. i have added the other 2 parts last night and tonight ill try pull it out the mould. 

There might be a issue with getting it out thou as i only did a layer of release , 2 wax coats then a layer of release.

So i can see myself redoing this one. 
 
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yeh those voids will cause you some problems if you don't fix them now. Multi-axial fabric isn't wonderful for the sort of shape you've got there, it does like to bridge. 

What weight fabrics did you use and how many layers? I think it might also be a bit light, you don't want your mould to be too flimsy. 
ChrisR
ChrisR
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
You've got a lot of voids / bridging going on there, you might want to fix them before you lay up the next few layers
MiggzFSU
MiggzFSU
Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)
Group: Forum Members
Posts: 7, Visits: 50
thanks for the help guys 

this is how im doing it, dont know if its right but suppose inn see once its done. 

im doing the face and the bottom mounts one piece, then the top and back in another piece 











then did the gel coat, did a thick layer let it get nearly dry and added another layer 





then added a light strand mat



then added another 2 layers of thick strand 

tonight ill me making the 2nd and 3rd mold sections 

 
MiggzFSU
MiggzFSU
Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)
Group: Forum Members
Posts: 7, Visits: 50
thank you so much i really appreciate the help 
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Definitely out of carbon. Just to clarify, you make the whole thing as one piece, including the brackets. You just make a split mould so that you can disassemble the mould around the mechanical locks. 

As for how many layers, is this a street or track only car? If it's track only, I'd just do one layer of 200g and one layer of 450g. Put an extra 2 layers of 450g on the brackets. 

If it's a street driven car, I'd advise a thickness of at least 3mm, and I would do that as a cored laminate. So one layer of 200g carbon, one layer of 3mm Soric or 3D PET Core (trim it just short of the edges of your part so it isn't exposed), and another layer 200g. Make the brackets solid carbon with no core, one layer 200 and 3 layers 450.
MiggzFSU
MiggzFSU
Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)
Group: Forum Members
Posts: 7, Visits: 50
perfect thanks mate 

would you make the brackets out of cf as well or would you make them out of metal? 

then next question, how many sheets of cr would one use?
Edited 9 Years Ago by MiggzFSU
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Pretty straight forward mate, main body of the fender is one piece, brackets will need barriers. You can probably make the top bracket and the main fender together, then the bottom bracket and the front and back brackets can be done separately. 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search