Hi all, 
Quick newbie question, am currently skinning some motorcycle parts in carbon and have a question, I have seen some people use easy composites fusionfix gp spray adhesive to stick the layer of carbon down, I have done it with a coat of epoxy and wait till tack as per the videos, just wondered if the fusionfix is better or is the layer of epoxy the way to go? pros/cons? 
Thanks in advance
Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
it's easier to reposition with the spray than epoxy, 
about the performance I'm not sure how much difference there will be,
I'm happy with the results with spraytack and always do it that way without any problems so far... matter of preference I think

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search