Hi just a quick question

I have read up and watched your tutorials but still a little unsure on how long I should leave the coupling coat and the light weight matt ply to cure before moving onto the main heavy plies with uni-mould tooling resin.

Regards
Ian
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
You can move on as soon as it is hard. 
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Hanaldo is essentially correct. The time it takes for the Coupling Coat to cure varies depending on the ambient temperature and the ratio of MEKP used so it is hard to give an accurate time frame. If you are in a hurry, I would come back after no more than 2 hours and keep checking from there until the resin is cured and ready for the backing plies.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Porkster0
Porkster0
Supreme Being (216 reputation)Supreme Being (216 reputation)Supreme Being (216 reputation)Supreme Being (216 reputation)Supreme Being (216 reputation)Supreme Being (216 reputation)Supreme Being (216 reputation)Supreme Being (216 reputation)Supreme Being (216 reputation)
Group: Forum Members
Posts: 14, Visits: 69
Hi Hanaldo and Warren

Thanks for the replys I am in no rush just didn't want to leave it too long !

so basically when it has hardened off it is ready to lay up,

Regards

ian
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
That is correct.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search