fjm9898
fjm9898
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 5,
Visits: 14
Resin Research 2050
Same stuff i have been using for the last year.
Reply
Like
7
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
What resin did you infuse with?
Reply
Like
8
fjm9898
fjm9898
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 5,
Visits: 14
I am not a happy camper today. I spent a bunch of money to have GC50 sent to the US because its the only thing that will work according to Easy Composites.
I followed every direction perfectly and soon as i cut the part, it start to chip up immediately.
I got the mixing portions right, i bought a spray gun. Laid it on a bit thinker, maybe 0.5mil or 0.6 mill, but should not of been a problem since some people brush it on heavier.
i let it stand for about 10 hours, well after the 2-3 cure time and well within the 24hour max out period. i did resin in fusion. i let the resin and the gc50 cure for 3 days. first cut, darn near instantly started to chip up and de-laminate. i used a cutoff wheel and actually moved downt eh part slow and moved fast to see if it was heat or speed, still happened no matter what.
i am at a loss guys. this product was supposed to be aon a show car tomorrow and i completely blew it because of this issue. i really dont understand.
here are a few pictures.
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
6
Prev
1
2
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search