Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
New Member Introductions
»
Hello from Ujezd, Czech Republic!
Hello from Ujezd, Czech Republic!
Post Reply
Like
5
Hello from Ujezd, Czech Republic!
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
ujezdan
ujezdan
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 6,
Visits: 110
Hi to everybody!
My name is Ondra,
I'm 25 years old and I'm from Czech Republic and I'm interested for composites about 3 years.
I work as a mechanical designer and I study long distance at University in Zlin with focus on composites. I did my bachelor thesis this year and my theme was:
Applying Vacuum Infusion for the Production of Hybrid Composite System
.
I send you some pictures of the result.
Working with composites is my hobby and I want to realize many projects - at University and at home too.
I want to learn more about this problematic and I want to share my knowledge.
Best regards,
Ondra
Attachments
13152640_10201684769158824_164801706_n.jpg
(
544 views,
81.00 KB
)
IMG_20160203_181753.jpg
(
558 views,
215.00 KB
)
13198570_10201699570368845_280744742703465671_o.jpg
(
557 views,
184.00 KB
)
Tags
Czech
Rally
S2000
Reply
Like
5
Reply
ujezdan
ujezdan
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 6,
Visits: 110
Thank you guys!
I write some info to the part: It was made with a vacuum infusion, 3 layers of 180g/m2 carbon fabric, no gelcoat.
Next time, in case of the same part I will do a few modification : Laminating by hand with a vacuum bag, I will use gelcoat.
I think that this technique will be faster with better result
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Hello from Ujezd, Czech Republic!
ujezdan
-
9 Years Ago
welcome aboard :)
tomzi1234
-
9 Years Ago
Welcome to the forum Ondra The bonnet /scuttle vent look like a complex part cutting out all those...
davro
-
9 Years Ago
Thank you guys! :) I write some info to the part: It was made with a vacuum infusion, 3 layers...
ujezdan
-
9 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search