Thanks guys, Sounds like I will be spraying it on. My question about the pva was not if it would de-mould well but if I spray it on the pva, will it lay right?
Guess I need to just wait tell it gets here and give it a shot. I want to have it on thiere thick enough I could do some minor sanding if needed.
im at the point were I am cuting back the amount of waxing I do,just 2 times then pva.
I can say coming from a noob I was using was to much, so much that the wax was efecting my part surface. NOW I know that just a haze of wax is al you need, otherwise more work later....
If Brute Force Isn''''t working your not using enough...
|