Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
I would as Fred says, check the accuracy of the gauge and also check thoroughly for leaks. The gauges can loose accuracy if impacted or dropped.
A good guide is to listen to the change of the pumps tone as it achieves near full vacuum. It should be a clear change. You can usually hear it more obviously if you shut the valve while the pump is working hard and see the difference.
If you are still struggling, then please get in contact and we will look further into it for you.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|