Hatvan Kilenc
Hatvan Kilenc
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 6,
Visits: 91
Hi all!
Any ideas how to construct an extremely durable plate (19,5 x 30 cm)? I have made few tests with different methods and the results have very promising but not good enough. The plate has to be so strong that it won´t break under a direct hit of an 170 g object hitting it in a speed of 180 km/h, impact energy will approx. 200 J. So far i have done plates from carbon and kevlar, few layers of carbon to give rigidity and to keep the plate in shape, in top few layers of kevlar to add strength. The question is should i put the kevlar only in top or also between carbon layers? Is 200 g carbon and kevlar strong enough? Should i put layers kevlar/carbon/kevlar/carbon/kevlar or kevlar/kevlar/carbon/carbon/kevlar on some other way? Plate will take hits only on the other side, so maybe more kevlar on that side? What about if i use some glass fibre instead of carbon fibre, Kevlar/kevlar/glass/carbon/glass?
Reply
Like
3
Fasta
Fasta
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 3.5K
I would say either all Kevlar or a mix of Kevlar and fibreglass.
Then it's just a matter of how thick?
Carbon fibre is kind of like an ultimate stiffness material but it will not take shock and impacts as well as Kevlar or fibre glass.
Fastacraft Facebook page
Reply
Like
3
D3O Phil
D3O Phil
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 22,
Visits: 498
That is quite an impact 170g at 50m/s
At those energies and velocities you will cause damage to anything therefore your 'plate' will be a one hit deal, I suspect your definitiaon of break should mean it won't penetrate through the plate to the other side?
is your object pointy or blunt? as this makes a big difference as to the impacted area and load spread meaning you could get away with a thinner layup
for what it's worth this sort of protection is typically 2 layers of fibre glass to create a rigid outer shell and approximately 15 layers of aramid behind to stop penetration.
Reply
Like
2
Hatvan Kilenc
Hatvan Kilenc
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 6,
Visits: 91
Thanks for answers, the object is ice hockey puck, so it won´t penetrate through (i hope
). Thickness should be (or can be) 2-3 mm.
Reply
Like
3
D3O Phil
D3O Phil
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 22,
Visits: 498
Ahh I wasn't expecting a hockey puck!
Have you thought about creating the puck as a spiral like a snail or liquorice wheel rather than in layers?
I suspect it might be more robust as you wouldn't be impacting the edges of the laminate
Reply
Like
3
Dravis
Dravis
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 592,
Visits: 1.9K
Gneek ...
I think you misunderstod the original poster .. Phil .. The Icehockey pPuck is the "projectile" -- What he wants to make is something that will stop the puck when fired at max velocity .. Because of the rather large and rounded "contact area" from the puck (The edges are the worst) What you need is something that is stiff enough to spread the impact over a larger area, so a combination of Kevlar and CF does not seem like such a bad idea ..
"Sapere Aude"... Dare to KNOW!
The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...
103% of all people do not understand statistics...
Do not adjust our mind, theres a fault in reality :-)
Reply
Like
3
D3O Phil
D3O Phil
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 22,
Visits: 498
Ah Doh!
The biggest factor for this would be the padding behind the plate then
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search