Newbie Question About Epoxy "Beading" in Mold


Author
Message
Tango
Tango
Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)
Group: Forum Members
Posts: 5, Visits: 14
Hi guys, sorry for the Newbie Question,  but this is really giving me some grief.
I made a mould with the Easy Composites mould kit, which came out really well, and I'm using wet lay to make parts from it. I've coated the mould with easylease, but when I put a coating of epoxy into it as a kind of gel coat the epoxy beads like water on a waxed car panel. I've tried using release wax and PVA release agent, but they all do the same thing. I did try a gel coat, which was slightly better as it was a bit thicker, but I had to keep brushing it until it had virtually cured to stop it leaving gaps. The part is going to be used near a motorbike engine, so I was using high temp epoxy, which has a longer cure time, so it's harder to keep brushing it to maintain the even coverage.
So, I'm at a loss to know what I'm doing wrong? The mould was thoroughly cleaned before applying the release agents. The part is cosmetic, so the finish is really important. 
Any ideas please?
Cheers.
Reply
Tango
Tango
Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)
Group: Forum Members
Posts: 5, Visits: 14
Many thanks for the advice guys. I've just received my next batch of materials, so the experimentation will continue!
I feel that I'm close to a solution.
With the High Temp epoxy I'm mixing the hardener at 35%, but would increasing this slightly hurt the finished product? 